Microtensile bond strength of lithium disilicate ceramics to resin adhesives.

The journal of adhesive dentistry (2014-12-18)
Moustafa N Aboushelib, Donia Sleem
要旨

To evaluate the influence of the internal structure of lithium disilicate glass ceramics (LDC) on the microtensile bond strength to a resin adhesive using two surface treatments. Milling blocks of three types of LDC were sectioned (4 mm thick) using a precision cutting machine: IPS Empress 2 (conventional LDC), IPSe.max CAD (a refined crystal high strength LDC), and Celtra (zirconia reinforced LDC). Cut specimens received crystallization heat treatment as suggested by the manufacturers. Two surface treatments were performed on each group: hydrofluoric acid etching (HF) and airborne particle abrasion using 50-μm glass beads, while the as-cut surface served as control. Treated surfaces were examined using scanning electron microscopy (SEM). The disks were coated with a silane primer and bonded to pre-aged resin composite disks (Tetric EvoCeram) using a resin adhesive (Variolink II) and then stored in water for 3 months. Bonded specimens were sectioned into micro-bars (1x1x6 mm) and microtensile bond strength test (MTBS) was performed. Data were analyzed using two-way ANOVA and Tukey's post-hoc test (α=0.05). Statistical analysis revealed significant differences in microtensile bond strength values between different LDCs (F=67, p<0.001), different surface treatments (F=232, p<0.001), and interaction between LDC and surface treatments (F=10.6, p<0.001). Microtensile bond strength of Celtra ceramic (30.4±4.6 MPa) was significantly higher than both IPS Empress 2 (21.5±5.9 MPa) and IPSe.max ceramics (25.8±4.8 MPa), which had almost comparable MTBS values. SEM images demonstrated homogenous glassy matrix and reinforcing zirconia fillers characteristic of Celtra ceramic. Heat treatment resulted in growth and maturation of lithium disilicate crystals. Particle abrasion resulted in abrasion of the glass matrix and exposure of lithium disilicate crystals, while HF etching produced a microrough surface, which resulted in higher MTBS values and reduction in the percentage of adhesive failure for all groups. Within the limitations of this study, bond strength to lithium disilicate ceramics depends on proper surface treatment and on the chemical composition of the glass ceramic.

材料
製品番号
ブランド
製品内容

Sigma-Aldrich
水, suitable for HPLC
Sigma-Aldrich
水, Nuclease-Free Water, for Molecular Biology
Sigma-Aldrich
水, sterile-filtered, BioReagent, suitable for cell culture
Sigma-Aldrich
水, HPLC Plus
Sigma-Aldrich
フッ化水素酸, ACS reagent, 48%
Sigma-Aldrich
水, Deionized
Sigma-Aldrich
水, for embryo transfer, sterile-filtered, BioXtra, suitable for mouse embryo cell culture
Sigma-Aldrich
フッ化水素酸, 48 wt. % in H2O, ≥99.99% trace metals basis
Sigma-Aldrich
水, for molecular biology, sterile filtered
Sigma-Aldrich
酸化ジルコニウム(IV), powder, 5 μm, 99% trace metals basis
Sigma-Aldrich
水, BioPerformance Certified
Sigma-Aldrich
酸化ジルコニウム(IV), nanopowder, <100 nm particle size (TEM)
Sigma-Aldrich
水, ACS reagent
Sigma-Aldrich
Distilled water
Sigma-Aldrich
水, for cell biology, sterile ultrafiltered
Sigma-Aldrich
ジルコニウム, powder, −100 mesh
Supelco
水, suitable for ion chromatography
Sigma-Aldrich
水, PCR Reagent
Sigma-Aldrich
水、重水素除去, ≤1 ppm (Deuterium oxide)
Sigma-Aldrich
酸化ジルコニウム(IV), 99.99% trace metals basis (purity excludes ~2% HfO2)
Sigma-Aldrich
ジルコニウム, foil, thickness 0.1 mm, 99.98% trace metals basis
Sigma-Aldrich
フッ化水素酸, 55%, CP
Supelco
水, for TOC analysis
Sigma-Aldrich
Distilled water, suitable for HPLC
Sigma-Aldrich
E-Toxate Water, endotoxin, free
Sigma-Aldrich
ジルコニウム, sponge, ≥99% trace metals basis
Supelco
水, ACS reagent, for ultratrace analysis
純水密度標準品, UKAS ISO/IEC17025 and ISO Guide 34 certified, density: 0.9982 g/mL at 20 °C, density: 0.9970 g/mL at 25 °C
Sigma-Aldrich
ジルコニウム, rod, diam. 6.35 mm, ≥99% trace metals basis
Sigma-Aldrich
酸化ジルコニウム(IV)分散液, nanoparticles, dispersion, <100 nm particle size (BET), 10 wt. % in H2O