詳細

heavy metal free

フォーム

beads

キャパシティ

>30 % absorption capacity (water)(at 80% rel. humidity, 25°C)

SMILES記法

[Si](=O)=O

InChI Key

VYPSYNLAJGMNEJ-UHFFFAOYSA-N

詳細

Drying pearls Orange (Silica gel orange), commonly used as a drying agent in laboratories, is suitable for drying all gases and solids. It is used in desiccators, drying towers, and absorption tubes. Silica gel orange provides longer storage conditions due to its large surface area which enables high absorption capacity. It also changes its color from orange to colorless after moisture absorption (approx. 6 wt% load).[1][2][3]

再構成

130~160°Cで乾燥することで再生します。160°C以上に加熱しないでください。

保管分類コード

13 - Non Combustible Solids

WGK

nwg

引火点(°F)

Not applicable

引火点(℃)

Not applicable

個人用保護具 (PPE)

Eyeshields, Gloves, type N95 (US)


適用法令

試験研究用途を考慮した関連法令を主に挙げております。化学物質以外については、一部の情報のみ提供しています。 製品を安全かつ合法的に使用することは、使用者の義務です。最新情報により修正される場合があります。WEBの反映には時間を要することがあるため、適宜SDSをご参照ください。

労働安全衛生法名称等を表示すべき危険物及び有害物

名称等を表示すべき危険物及び有害物

労働安全衛生法名称等を通知すべき危険物及び有害物

名称等を通知すべき危険物及び有害物

Jan Code

94098-1KG:
94098-500G:
94098-VAR:
94098-BULK:


最新バージョンのいずれかを選択してください:

試験成績書(COA)

Lot/Batch Number

適切なバージョンが見つかりませんか。

特定のバージョンが必要な場合は、ロット番号またはバッチ番号で特定の証明書を検索できます。

以前この製品を購入いただいたことがある場合

文書ライブラリで、最近購入した製品の文書を検索できます。

文書ライブラリにアクセスする

この製品を見ている人はこちらもチェック

Slide 1 of 3

1 of 3

M Zabeti et al.
Bioresource technology, 118, 374-381 (2012-06-19)
Canadian pinewood was pyrolyzed at 450 °C in an Infrared oven and the pyrolysis vapors were converted by passing through a catalyst bed at 450 °C. The catalysts studied were amorphous silica alumina (ASA) containing alkali metal or alkaline earth
Georgios Toskas et al.
ACS applied materials & interfaces, 3(9), 3673-3681 (2011-08-24)
Ceramic silica (SiO(2)) hybrid nanofibers were prepared by electrospinning of solutions containing biocompatible polymer and modified silica precursors. The new hybrid nanofibers are based on polyethylene oxide (PEO) and a new solution of modified sol-gel particles of mixture containing tetraethoxysilane
Jamieson K Christie et al.
The journal of physical chemistry. B, 116(41), 12614-12620 (2012-09-18)
The low solubility (high durability) of yttrium aluminosilicate (YAS) glass is one of its most important properties for use in in situ radiotherapy. Simple parameters, such as silica or yttria content or network connectivity, are not sufficient to rationalize the
Proton conductivity in silica gels
Schober T
Ionics, 12(2), 131-134 (2006)
Dun-Yen Kang et al.
ACS applied materials & interfaces, 4(2), 965-976 (2012-01-21)
The fabrication, detailed characterization, and molecular transport properties of nanocomposite membranes containing high fractions (up to 40 vol %) of individually-dispersed aluminosilicate single-walled nanotubes (SWNTs) in poly(vinyl alcohol) (PVA), are reported. The microstructure, SWNT dispersion, SWNT dimensions, and intertubular distances

質問

1–3/3 質問  
  1. How is shipping temperature determined? And how is it related to the product storage temperature?

    1 回答
    1. Products may be shipped at a different temperature than the recommended long-term storage temperature. If the product quality is sensitive to short-term exposure to conditions other than the recommended long-term storage, it will be shipped on wet or dry-ice. If the product quality is NOT affected by short-term exposure to conditions other than the recommended long-term storage, it will be shipped at ambient temperature. As shipping routes are configured for minimum transit times, shipping at ambient temperature helps control shipping costs for our customers. For more information, please refer to the Storage and Transport Conditions document: https://www.sigmaaldrich.com/deepweb/assets/sigmaaldrich/marketing/global/documents/316/622/storage-transport-conditions-mk.pdf

      役に立ちましたか?

  2. How can I determine the shelf life / expiration / retest date of this product?

    1 回答
    1. If this product has an expiration or retest date, it will be shown on the Certificate of Analysis (COA, CofA). If there is no retest or expiration date listed on the product's COA, we do not have suitable stability data to determine a shelf life. For these products, the only date on the COA will be the release date; a retest, expiration, or use-by-date will not be displayed.
      For all products, we recommend handling per defined conditions as printed in our product literature and website product descriptions. We recommend that products should be routinely inspected by customers to ensure they perform as expected.
      For products without retest or expiration dates, our standard warranty of 1 year from the date of shipment is applicable.
      For more information, please refer to the Product Dating Information document: https://www.sigmaaldrich.com/deepweb/assets/sigmaaldrich/marketing/global/documents/449/386/product-dating-information-mk.pdf

      役に立ちましたか?

  3. Bonjour, quelle est la couleur des perles quand c'est sec et quand c’est humide? Quelle est la température et le temps nécessaire pour régénérer ces perles? Merci d'avance!

    1 回答
    1. This material changes its color from orange to colorless after moisture absorption (approx. 6 wt% load). The protocol for the regeneration is to spread the beads in a thin layer (max 10 mm) in a oven tray, preheat the oven at 110-130C, dry the beads for 90 minutes (or more if after 90 minutes the color is not orange again), and let them cool and place in a airtight container.

      役に立ちましたか?

レビュー

評価値なし

アクティブなフィルタ

ライフサイエンス、有機合成、材料科学、クロマトグラフィー、分析など、あらゆる分野の研究に経験のあるメンバーがおります。.

製品に関するお問い合わせはこちら(テクニカルサービス)