推薦產品
等級
purum p.a.
化驗
≥96.0% (calc. as Ca3(PO4)2, KT)
形狀
powder
損耗
≤0.1% loss on ignition, 800 °C
負離子痕跡
chloride (Cl-): ≤500 mg/kg
sulfate (SO42-): ≤1000 mg/kg
正離子痕跡
Cd: ≤50 mg/kg
Co: ≤50 mg/kg
Cu: ≤50 mg/kg
Fe: ≤200 mg/kg
K: ≤500 mg/kg
Na: ≤1000 mg/kg
Ni: ≤50 mg/kg
Pb: ≤50 mg/kg
Zn: ≤50 mg/kg
SMILES 字串
[Ca++].[Ca++].[Ca++].[O-]P([O-])([O-])=O.[O-]P([O-])([O-])=O
InChI
1S/3Ca.2H3O4P/c;;;2*1-5(2,3)4/h;;;2*(H3,1,2,3,4)/q3*+2;;/p-6
InChI 密鑰
QORWJWZARLRLPR-UHFFFAOYSA-H
尋找類似的產品? 前往 產品比較指南
儲存類別代碼
11 - Combustible Solids
水污染物質分類(WGK)
WGK 1
閃點(°F)
Not applicable
閃點(°C)
Not applicable
客戶也查看了
S Leeuwenburgh et al.
Journal of biomedical materials research, 56(2), 208-215 (2001-05-08)
A new biomimetic method for coating metal implants enables the fast formation of dense and homogeneous calcium phosphate coatings. Titanium alloy (Ti6Al4V) disks were coated with a thin, carbonated, amorphous calcium phosphate (ACP) by immersion in a saturated solution of
Calcium phosphates compounds in conjunction with hydrogel as carrier for BMP-2: a study on ectopic bone formation in rats.
Hulsart-Billstrom G, et al.
Acta Biomaterialia, 7(8), 3042-3049 (2011)
Calcium phosphate-based osteoinductive materials.
LeGeros RZ.
Chemical Reviews, 108(11), 4742-4753 (2008)
3D printing of bone substitute implants using calcium phosphate and bioactive glasses.
Bergmann C, et al.
J. Eur. Ceram. Soc., 30(12), 2563-2563 (2010)
S I Roohani-Esfahani et al.
Acta biomaterialia, 8(11), 4162-4172 (2012-07-31)
This is the first reported study to prepare highly porous baghdadite (Ca₃ZrSi₂O₉) scaffolds with and without surface modification and investigate their ability to repair critical-sized bone defects in a rabbit radius under normal load. The modification was carried out to