跳转至内容
Merck

85419

Sigma-Aldrich

硅油 AR 200

viscosity ~200 mPa.s,   neat(25 °C)

别名:

聚苯基-甲基硅氧烷

登录查看公司和协议定价


About This Item

CAS号:
MDL號碼:
分類程式碼代碼:
12352103
NACRES:
NA.22

形狀

oil

折射率

n20/D 1.453

黏度

~200 mPa.s, neat(25 °C)

密度

1.05 g/mL at 20 °C

相关类别

一般說明

硅油AR 200是一种带苯基的聚二甲基硅氧烷,通常用作热传导或压力传导流体。

應用

硅油AR 200可用作:
  • 一种化学改性剂,以用于改性热固性酚醛树脂,以制备胶粘剂。
  • 4′-正辛基-4-氰基-联苯液晶基质的掺杂剂。

特點和優勢

特别好的热稳定性

儲存類別代碼

10 - Combustible liquids

水污染物質分類(WGK)

WGK 3

閃點(°F)

545.0 °F

閃點(°C)

285 °C

個人防護裝備

Eyeshields, Gloves


分析证书(COA)

输入产品批号来搜索 分析证书(COA) 。批号可以在产品标签上"批“ (Lot或Batch)字后找到。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

其他客户在看

C Eckardt et al.
Ophthalmologica. Journal international d'ophtalmologie. International journal of ophthalmology. Zeitschrift fur Augenheilkunde, 201(3), 133-139 (1990-01-01)
Different methylphenylsilicone (MPS) and fluorosilicone (FS) oils having a higher specific gravity than water were investigated as vitreous replacements. Their intraocular tolerance in vitrectomized aphakic rabbit eyes was evaluated for periods of up to 4 months and compared to that
O Gyllenhaal et al.
Journal of chromatography, 516(2), 415-426 (1990-09-21)
The supercritical fluid chromatography of intact aliphatic amines with different columns is described. One group of amines was based on N,N-dimethyl-n-octylamine and related primary and secondary amines, and the other on the amino alcohol metoprolol and several of its analogues.
Experience with a silicone resin (polymethylphenylsiloxane) hard contact lens.
H Magatani et al.
The CLAO journal : official publication of the Contact Lens Association of Ophthalmologists, Inc, 9(3), 261-266 (1983-07-01)
H Kriegs et al.
The Journal of chemical physics, 124(10), 104901-104901 (2006-03-18)
In some polymers, in addition to the usual structural alpha relaxation, a slower alpha' relaxation is observed with a non-Arrhenius temperature dependence. In order to understand better the molecular origin of this alpha' relaxation in poly(methylphenylsiloxane) (PMPS) we have studied
G B Chen et al.
Se pu = Chinese journal of chromatography, 18(4), 343-345 (2003-01-25)
An insoluble beta-cyclodextrin polymer cross-linked with epichlorohydrin was prepared. beta-Cyclodextrin polymer (0.26 g) was treated for 0.5 h by a ultrasonator in the mixed solvent (10 mL) of isopropyl ether, methylene dichloride and benzene with a volume ratio 2:1:2, and

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门