GF78786354
Tantalum
foil, 25x25mm, thickness 0.25mm, annealed, 99.99%
Sinônimo(s):
Tantalum, TA000472, Ta
Faça loginpara ver os preços organizacionais e de contrato
About This Item
pressão de vapor
<0.01 mmHg ( 537.2 °C)
Ensaio
99.99%
forma
foil
temperatura de autoignição
572 °F
fabricante/nome comercial
Goodfellow 787-863-54
resistividade
13.5 μΩ-cm, 20°C
tamanho × espessura
25 x 25 mm × 0.25 mm
pb
5425 °C (lit.)
pf
2996 °C (lit.)
densidade
16.69 g/cm3 (lit.)
cadeia de caracteres SMILES
[Ta]
InChI
1S/Ta
chave InChI
GUVRBAGPIYLISA-UHFFFAOYSA-N
Descrição geral
For updated SDS information please visit www.goodfellow.com.
Informações legais
Product of Goodfellow
Certificados de análise (COA)
Busque Certificados de análise (COA) digitando o Número do Lote do produto. Os números de lote e remessa podem ser encontrados no rótulo de um produto após a palavra “Lot” ou “Batch”.
Já possui este produto?
Encontre a documentação dos produtos que você adquiriu recentemente na biblioteca de documentos.
Radiation research, 165(4), 452-459 (2006-04-04)
We determined effective cross sections for production of single-strand breaks (SSBs) in plasmid DNA [pGEM 3Zf(-)] by electrons of 10 eV and energies between 0.1 and 4.7 eV. After purification and lyophilization on a chemically clean tantalum foil, dry plasmid
Applied optics, 31(22), 4397-4404 (1992-08-01)
A simple four-element fused-silica lens is presented that has a focal length of 31.2 mm and a relative aperture of f/1 for use as a focusing lens for deep UV laser processing. The curvature of the lens is designed with
Tantalum foil pegs.
American journal of ophthalmology, 34(3), 444-444 (1951-03-01)
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
Nossa equipe de cientistas tem experiência em todas as áreas de pesquisa, incluindo Life Sciences, ciência de materiais, síntese química, cromatografia, química analítica e muitas outras.
Entre em contato com a assistência técnica