GF87282254

foil, 6mm disks, thickness 0.01mm, 99.9%

同義詞:

登入查看組織和合約定價


About This Item

經驗公式(希爾表示法):
Zn
CAS號碼:
分子量::
65.39
MDL號碼:
分類程式碼代碼:
12141750
PubChem物質ID:
NACRES:
NA.23

蒸汽壓力

1 mmHg ( 487 °C)

化驗

≥99.9%

形狀

foil

製造商/商標名

Goodfellow 872-822-54

電阻係數

5.8 μΩ-cm, 20°C

bp

907 °C (lit.)

mp

420 °C (lit.)

密度

7.133 g/mL at 25 °C (lit.)

SMILES 字串

[Zn]

InChI

1S/Zn

InChI 密鑰

HCHKCACWOHOZIP-UHFFFAOYSA-N

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

從最近期的版本中選擇一個:

分析證明 (COA)

Lot/Batch Number

抱歉,我們目前沒有在線上提供本產品的COA

如果您需要協助,請聯絡 客戶支援

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

A new vapor-phase hydrothermal method to concurrently grow ZnO nanotube and nanorod array films on different sides of a zinc foil substrate.
Haimin Zhang et al.
Chemistry (Weinheim an der Bergstrasse, Germany), 18(17), 5165-5169 (2012-03-21)
S Rondot et al.
Science (New York, N.Y.), 263(5154), 1739-1741 (1994-03-25)
An x-ray projection microscope equipped with a charge-coupled device camera allows direct observation of zinc (Zn(2+)) ions diffusing in aqueous hydrochloric acid solution during the corrosion of zinc foil and pellets. Time series of microradiographic images with a lateral resolution
Tandra Ghoshal et al.
Journal of nanoscience and nanotechnology, 9(9), 5586-5591 (2009-11-26)
Nanowire arrays of zinc oxide were synthesized on zinc foil by a simple thermal evaporation process. Morphologies and sizes of the synthesized nanostructures were varied by varying the reaction time and the surface roughness of the substrate. Self-catalytic liquid-solid mechanism
Chenglin Yan et al.
The journal of physical chemistry. B, 110(51), 25850-25855 (2006-12-22)
Vertically aligned ZnO nanorods with uniform diameter and length have been synthesized on a zinc foil substrate with ammonium persulfate as oxidant via a facile, larger scale production and inexpensively synthesized method without any templates or additives. SEM and XRD
Xufeng Wu et al.
Chemical communications (Cambridge, England), (15)(15), 1655-1657 (2006-04-04)
Highly oriented ZnO nanoneedle/nanorods arrays have been fabricated by direct oxidation of zinc foil in alkaline zincate ion solution at near room temperature (20 degrees C for nanoneedles, 30 degrees C for nanorods).

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務