跳轉至內容
Merck
全部照片(2)

文件

GF80180377

foil, 4mm disks, thickness 0.006mm, 99.9%

同義詞:

钽, Ta

登入查看組織和合約定價


About This Item

經驗公式(希爾表示法):
Ta
CAS號碼:
分子量::
180.95
MDL號碼:
分類程式碼代碼:
12141741
PubChem物質ID:
NACRES:
NA.23

蒸汽壓力

<0.01 mmHg ( 537.2 °C)

化驗

99.9%

形狀

foil

自燃溫度

572 °F

製造商/商標名

Goodfellow 801-803-77

電阻係數

13.5 μΩ-cm, 20°C

直徑× 厚度

4 mm × 0.006 mm

bp

5425 °C (lit.)

mp

2996 °C (lit.)

密度

16.69 g/cm3 (lit.)

SMILES 字串

[Ta]

InChI

1S/Ta

InChI 密鑰

GUVRBAGPIYLISA-UHFFFAOYSA-N

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

分析證明 (COA)

輸入產品批次/批號來搜索 分析證明 (COA)。在產品’s標籤上找到批次和批號,寫有 ‘Lot’或‘Batch’.。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

Radmila Panajotovic et al.
Radiation research, 165(4), 452-459 (2006-04-04)
We determined effective cross sections for production of single-strand breaks (SSBs) in plasmid DNA [pGEM 3Zf(-)] by electrons of 10 eV and energies between 0.1 and 4.7 eV. After purification and lyophilization on a chemically clean tantalum foil, dry plasmid
Yingxun Du et al.
Journal of hazardous materials, 225-226, 21-27 (2012-05-23)
In order to overcome the limitation of the application of nanoparticles, tantalum (oxy)nitrides nanotube arrays on a Ta foil were synthesized and introduced in vis (visible light)-Fenton-like system to enhance the degradation of atrazine. At first, the anodization of tantalum
Zhongli Cai et al.
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
T Y Hung et al.
Applied optics, 31(22), 4397-4404 (1992-08-01)
A simple four-element fused-silica lens is presented that has a focal length of 31.2 mm and a relative aperture of f/1 for use as a focusing lens for deep UV laser processing. The curvature of the lens is designed with
Zhongli Cai et al.
Radiation research, 165(3), 365-371 (2006-02-24)
Both thick and thin films of pGEMR-3Zf- plasmid DNA deposited on a tantalum foil were exposed to soft X rays (effective energy of 14.8 keV) for various times in air under a relative humidity of 45% (Gamma approximately 6, where

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務