推荐产品
蒸汽壓力
<0.01 mmHg ( 537.2 °C)
化驗
≥99% trace metals basis
形狀
nanopowder
自燃溫度
572 °F
電阻係數
13.5 μΩ-cm, 20°C
粒徑
<25 nm (BET)
bp
5425 °C (lit.)
mp
2996 °C (lit.)
密度
16.69 g/cm3 (lit.)
SMILES 字串
[Ta]
InChI
1S/Ta
InChI 密鑰
GUVRBAGPIYLISA-UHFFFAOYSA-N
一般說明
超细颗粒的大量附聚体。
訊號詞
Danger
危險聲明
危險分類
Flam. Sol. 1
儲存類別代碼
4.1B - Flammable solid hazardous materials
水污染物質分類(WGK)
nwg
閃點(°F)
Not applicable
閃點(°C)
Not applicable
其他客户在看
International journal of nanomedicine, 15, 2419-2435 (2020-05-06)
In recent years, nanomaterials have been increasingly developed and applied in the field of bone tissue engineering. However, there are few studies on the induction of bone regeneration by tantalum nanoparticles (Ta NPs) and no reports on the effects of
Nanoscale, 5(4), 1494-1498 (2013-01-23)
Ta oxide nanotubes (NTs) were formed by the anodization of Ta at 15 V in a solution of concentrated sulfuric acid containing 0.8-1.0 M hydrofluoric acid. To study the initial stages of NT formation, FESEM images of samples anodized for
Orbital ultrasound in the selective screening of a dural-cavernous sinus fistula.
European journal of emergency medicine : official journal of the European Society for Emergency Medicine, 20(2), 137-139 (2013-02-26)
Journal of the mechanical behavior of biomedical materials, 16, 21-28 (2012-11-10)
Microstructure and mechanical properties of laser deposited complex quaternary Ti-34Nb-7Zr-7Ta (all wt%), an orthopedic load-bearing implant alloy, has been investigated in detail in both as-deposited as well as heat-treated (β-solutionized and quenched) conditions. The difference in stress-strain behavior of this
Vascular, 21(2), 87-91 (2013-03-20)
Control of back bleeding from the hypogastric artery into the aneurysm after endovascular aneurysm repair (EVAR) of a ruptured aorto-iliac aneurysm may be necessary in order to avoid a type II endoleak. It is an emergency situation and selective catheterization
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.
联系技术服务部门