跳转至内容
Merck

30620

Sigma-Aldrich

氢氧化钠

puriss. p.a., ACS reagent, reag. Ph. Eur., K ≤0.02%, ≥98%, pellets

别名:

‘苛性钠’

登录查看公司和协议定价


About This Item

线性分子式:
NaOH
CAS号:
分子量:
40.00
EC號碼:
MDL號碼:
分類程式碼代碼:
12352302
PubChem物質ID:
NACRES:
NA.21

等級

ACS reagent
puriss. p.a.

品質等級

agency

reag. Ph. Eur.

蒸汽密度

>1 (vs air)

蒸汽壓力

<18 mmHg ( 20 °C)
3 mmHg ( 37 °C)

化驗

≥98%

形狀

pellets

技術

titration: suitable

雜質

≤0.0003% total nitrogen (N)
≤0.0005% heavy metals (as Pb)
≤1% Na2CO3

mp

318 °C (lit.)

溶解度

water: soluble 1260 g/L at 20 °C

密度

2.13 g/cm3 at 20 °C

負離子痕跡

chloride (Cl-): ≤10 mg/kg
phosphate (PO43-): ≤5 mg/kg
silicate (as SiO2): ≤10 mg/kg
sulfate (SO42-): ≤30 mg/kg

正離子痕跡

Al: ≤5 mg/kg
As: ≤1 mg/kg
Ca: ≤5 mg/kg
Cu: ≤5 mg/kg
Fe: ≤5 mg/kg
Hg: ≤0.05 mg/kg
K: ≤200 mg/kg
Mg: ≤5 mg/kg
Ni: ≤5 mg/kg
Pb: ≤2 mg/kg
Zn: ≤5 mg/kg

儲存溫度

15-25°C

SMILES 字串

[OH-].[Na+]

InChI

1S/Na.H2O/h;1H2/q+1;/p-1

InChI 密鑰

HEMHJVSKTPXQMS-UHFFFAOYSA-M

正在寻找类似产品? 访问 产品对比指南

一般說明

氢氧化钠是无机碱。它参与由 Au/木炭或 Au/石墨催化的甘油氧化。它还参与无溶剂羟醛缩合反应。

應用

氢氧化钠可用于通过滴定测定胶体二氧化硅的比表面积。它可用于硼氢化钠的直接氧化,其通过循环和线性伏安法、计时电流法和计时电位法进行研究。它可用于组成柠檬酸盐缓冲液和硼酸盐缓冲液。
它可用于以下化合物的合成:
  • 烷基芳基氨基磺基甜菜碱
  • 3-[4-辛基苯氧基乙氧基乙氧基乙基]二甲基氨基丙磺酸盐(XOSB)
  • 三磺基甜菜碱(TriSBn)

象形圖

Corrosion

訊號詞

Danger

危險聲明

危險分類

Eye Dam. 1 - Met. Corr. 1 - Skin Corr. 1A

儲存類別代碼

8A - Combustible corrosive hazardous materials

水污染物質分類(WGK)

WGK 1

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析证书(COA)

输入产品批号来搜索 分析证书(COA) 。批号可以在产品标签上"批“ (Lot或Batch)字后找到。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

其他客户在看

Chemoselective, solvent-free aldol condensation reaction.
Raston CL and Scott JL.
Green Chemistry, 2(2), 49-52 (2000)
Kinetics of sodium borohydride direct oxidation and oxygen reduction in sodium hydroxide electrolyte: Part I. BH4- electro-oxidation on Au and Ag catalysts.
Chatenet M, et al.
Electrochimica Acta, 51(25), 5459-5467 (2006)
M A Roberts et al.
Analytical chemistry, 69(11), 2035-2042 (1997-06-01)
This report describes a UV laser photoablation method for the production of miniaturized liquid-handling systems on polymer substrate chips. The fabrication of fluid channel and reservoir networks is accomplished by firing 200 mJ pulses from an UV excimer laser at
Silvio Carrettin et al.
Chemical communications (Cambridge, England), (7)(7), 696-697 (2002-07-18)
Glycerol is oxidised to glyceric acid with 100% selectivity using either 1% Au/charcoal or 1% Au/graphite catalyst under mild reaction conditions (60 degrees C, 3 h, water as solvent).
Determination of specific surface area of colloidal silica by titration with sodium hydroxide.
Sears Jr GW.
Analytical Chemistry, 28(12), 1981-1983 (1956)

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门