推荐产品
分子量
average Mn ~300
转变温度
softening point 10 °C
密度
1.07 g/mL at 25 °C
正在寻找类似产品? 访问 产品对比指南
应用
聚己内酯三醇(PCL-三醇)可用于制备具有柠檬酸的可生物降解的弹性体,用于软组织工程应用。大量研究报告了 PCL-三醇用于制备在生物医学植入物中有多种用途的可生物降解聚氨酯。
储存分类代码
10 - Combustible liquids
WGK
WGK 1
闪点(°F)
424.4 °F - closed cup
闪点(°C)
218 °C - closed cup
个人防护装备
Eyeshields, Gloves
其他客户在看
Evaluation of in situ curable biodegradable polyurethanes containing zwitterion components.
Adhikari R, et al.
Journal of Materials Science. Materials in Medicine, 21(4), 1081-1089 (2010)
Synthetic and tissue-derived models for studying rigidity effects on invadopodia activity.
Methods in Molecular Biology (2013)
Processing and characterization of elastomeric polycaprolactone triol?citrate coatings for biomedical applications.
Shirazi H S, et al.
Progress in Organic Coatings, 77(4), 821-829 (2014)
(Citric acid?co?polycaprolactone triol) polyester: A biodegradable elastomer for soft tissue engineering.
Thomas L V and Nair P D
Biomatter, 1(1), 81-90 (2011)
商品
In the past two decades, tissue engineering and regenerative medicine have become important interdisciplinary fields that span biology, chemistry, engineering, and medicine.
Innovations in polymer technology have had a significant impact on the advancement of novel drug delivery systems.
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.