262919
Tantalum
foil, thickness 0.025 mm, ≥99.9% trace metals basis
Synonyme(s) :
Ta
Se connecterpour consulter vos tarifs contractuels et ceux de votre entreprise/organisme
About This Item
Produits recommandés
Pression de vapeur
<0.01 mmHg ( 537.2 °C)
Niveau de qualité
Essai
≥99.9% trace metals basis
Forme
foil
Température d'inflammation spontanée
572 °F
Résistivité
13.5 μΩ-cm, 20°C
Épaisseur
0.025 mm
pb
5425 °C (lit.)
Pf
2996 °C (lit.)
Densité
16.69 g/cm3 (lit.)
Chaîne SMILES
[Ta]
InChI
1S/Ta
Clé InChI
GUVRBAGPIYLISA-UHFFFAOYSA-N
Catégories apparentées
Description générale
The structure of tantalum is body centered cubic (BCC) metal. It is a refractory metal; stable up to very high temperatures. Tantalum is ductile at room temperature and moderately ductile at cryogenic temperatures.
Quantité
150 × 150 mm (appoximately 9 g)
150 × 500 mm (approximately 31 g)
150 × 500 mm (approximately 31 g)
Code de la classe de stockage
11 - Combustible Solids
Classe de danger pour l'eau (WGK)
nwg
Point d'éclair (°F)
Not applicable
Point d'éclair (°C)
Not applicable
Équipement de protection individuelle
Eyeshields, Gloves, type N95 (US)
Faites votre choix parmi les versions les plus récentes :
Déjà en possession de ce produit ?
Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.
Les clients ont également consulté
The Morphology of Tensile Failure in Tantalum
Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 44(10), 4567-4580 (2013)
International journal of molecular medicine, 31(3), 689-697 (2013-01-23)
Titanium (Ti) alloys of the β-type are highly attractive metallic materials for biomedical applications due to their low elastic modulus, high corrosion resistance and notable biocompatibility. A new β-type Ti35Nb2Ta3Zr alloy with a low Young's modulus of approximately 48 GPa was previously
Journal of neurosurgery. Spine, 18(6), 606-610 (2013-04-23)
Presurgical devascularization of hypervascular spinal metastases has been shown to be effective in preventing major blood loss during open surgery. Most often, embolization can be performed using polyvinyl alcohol (PVA) microparticles. However, in some cases, the close relationship between the
Biomimetic oxygen activation by MoS2/Ta3N5 nanocomposites for selective aerobic oxidation.
Angewandte Chemie (International ed. in English), 51(47), 11740-11744 (2012-10-17)
Journal of shoulder and elbow surgery, 22(4), 535-541 (2012-09-11)
Aseptic loosening of all-polyethylene glenoid components remains a limiting factor in achieving long-term implant survival in total shoulder arthroplasty (TSA). This study prospectively evaluated the functional and radiographic outcomes of patients undergoing TSA with a novel, porous, tantalum-backed glenoid component
Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..
Contacter notre Service technique