Passa al contenuto
Merck
Tutte le immagini(2)

Key Documents

GF45010369

Tin

foil, light tested, 25x25mm, thickness 0.02mm, 99.75%

Sinonimo/i:

Tin, SN000180

Autenticatiper visualizzare i prezzi riservati alla tua organizzazione & contrattuali


About This Item

Formula empirica (notazione di Hill):
Sn
Numero CAS:
Peso molecolare:
118.71
Numero MDL:
Codice UNSPSC:
12141745
ID PubChem:
NACRES:
NA.23

Saggio

99.75%

Forma fisica

foil

Produttore/marchio commerciale

Goodfellow 450-103-69

Resistività

11 μΩ-cm, 20°C

P. eboll.

2270 °C (lit.)

Punto di fusione

231.9 °C (lit.)

Densità

7.310 g/mL at 25 °C (lit.)

Stringa SMILE

[Sn]

InChI

1S/Sn
ATJFFYVFTNAWJD-UHFFFAOYSA-N

Descrizione generale

For updated SDS information please visit www.goodfellow.com.

Note legali

Product of Goodfellow

Certificati d'analisi (COA)

Cerca il Certificati d'analisi (COA) digitando il numero di lotto/batch corrispondente. I numeri di lotto o di batch sono stampati sull'etichetta dei prodotti dopo la parola ‘Lotto’ o ‘Batch’.

Possiedi già questo prodotto?

I documenti relativi ai prodotti acquistati recentemente sono disponibili nell’Archivio dei documenti.

Visita l’Archivio dei documenti

V G Shlopov et al.
Arkhiv patologii, 46(2), 80-81 (1984-01-01)
The quality of paraffin sections is determined to a considerable degree by the properties of paraffin block such as crystal size and spatial homogeneity. A new temperature regimen of treatment in preparation of paraffin blocks has been developed. After impregnation
K-H Utz et al.
Journal of oral rehabilitation, 29(5), 458-466 (2002-05-25)
In a dentate subject a jaw relation can either be determined in maximum intercuspation and is as such given by the occlusal morphology, or the mandibular position can be allocated according to the centric position of the condyles. For comprehensive
Andrey A Gurtovenko et al.
The Journal of chemical physics, 130(21), 215107-215107 (2009-06-11)
The electrostatic properties of lipid membranes are of profound importance as they are directly associated with membrane potential and, consequently, with numerous membrane-mediated biological phenomena. Here we address a number of methodological issues related to the computation of the electrostatic
Mercury contamination removed with tin foil.
R Grajower et al.
Operative dentistry, 9(3), 101-104 (1984-01-01)
Lis Danielsen et al.
Forensic science international, 134(2-3), 134-141 (2003-07-10)
Previously, electrical injuries have been suggested caused only by the concomitant heat developed during the passage of an electrical current. Recent experimental studies on fully anesthetized pigs and the study of one human case have, however, shown typical electrical alterations.

Il team dei nostri ricercatori vanta grande esperienza in tutte le aree della ricerca quali Life Science, scienza dei materiali, sintesi chimica, cromatografia, discipline analitiche, ecc..

Contatta l'Assistenza Tecnica.