267554
Tungsten
wire, diam. 0.25 mm, ≥99.9% trace metals basis
Synonym(s):
W
Sign Into View Organizational & Contract Pricing
All Photos(1)
About This Item
Recommended Products
Assay
≥99.9% trace metals basis
form
wire
resistivity
4.9 μΩ-cm, 20°C
diam.
0.25 mm
bp
5660 °C (lit.)
mp
3410 °C (lit.)
density
19.3 g/mL at 25 °C (lit.)
SMILES string
[W]
InChI
1S/W
InChI key
WFKWXMTUELFFGS-UHFFFAOYSA-N
Related Categories
Application
Tungsten (W) wire can be used for a variety of applications such as:
- fabrication of tungsten tips which can be used as field emitters, nanoprobes and scanning tunneling microscope (STM) probes.
- increase of the band gap of amorphous silicon germanium alloy.
- formation of tungsten fibers for potential usage in the lighting industry.
Quantity
9.5 g = 10 m; 95 g = 100 m
Storage Class Code
11 - Combustible Solids
WGK
nwg
Flash Point(F)
Not applicable
Flash Point(C)
Not applicable
Personal Protective Equipment
dust mask type N95 (US), Eyeshields, Gloves
Certificates of Analysis (COA)
Search for Certificates of Analysis (COA) by entering the products Lot/Batch Number. Lot and Batch Numbers can be found on a product’s label following the words ‘Lot’ or ‘Batch’.
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Customers Also Viewed
Recrystallization of tungsten wire for fabrication of sharp and stable nanoprobe and field-emitter tips
The Review of Scientific Instruments, 78(2), 026104-026104 (2007)
Improving narrow bandgap a-SiGe: H alloys grown by hot-wire chemical vapor deposition
Thin Solid Films, 430(1-2), 197-201 (2003)
Tungsten fibre-reinforced composites for advanced plasma facing components
Nuclear Materials and Energy, 12(1-2), 1308-1313 (2017)
Free radical biology & medicine, 41(9), 1353-1360 (2006-10-07)
Hyperlipidemia enhances xanthine oxidase (XO) activity. XO is an important source of reactive oxygen species (ROS). Since ROS are thought to promote atherosclerosis, we hypothesized that XO is involved in the development of atherosclerosis. ApoE(-/-) mice were fed a Western-type
Advanced materials (Deerfield Beach, Fla.), 25(14), 2095-2100 (2013-02-22)
A new photothermal coupling agent for photothermal ablation (PTA) therapy of tumors is developed based on ultrathin PEGylated W18O49 nanowires. After being injected with the nanowire solution, the in vivo tumors exhibit a rapid temperature rise to 50.0 ± 0.5
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service