蒸汽压
10 mmHg ( 0 °C)
方案
99-100.5% (complexometric)
质量
meets analytical specification of DAC, BPC
杂质
≤0.5% insoluble in acetic acid
缺失
≤0.2% loss on ignition, 700 °C
颜色
yellow
mp
886 °C (lit.)
痕量阴离子
chloride (Cl-): ≤50 mg/kg
痕量阳离子
Fe: ≤50 mg/kg
SMILES字符串
O=[PbH2]
InChI
1S/O.Pb
InChI key
YEXPOXQUZXUXJW-UHFFFAOYSA-N
正在寻找类似产品? 访问 产品对比指南
警示用语:
Danger
危险分类
Acute Tox. 4 Inhalation - Acute Tox. 4 Oral - Aquatic Acute 1 - Aquatic Chronic 1 - Carc. 2 - Lact. - Repr. 1A - STOT RE 1
靶器官
Central nervous system,Kidney,Blood
储存分类代码
6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects
WGK
WGK 3
闪点(°F)
Not applicable
闪点(°C)
Not applicable
Eagleson M.
Concise Encyclopedia Chemistry, 590-590 (1994)
Guoting Li et al.
Journal of environmental sciences (China), 23(6), 998-1003 (2011-11-10)
Beta-PbO2 electrodes were prepared by electro-deposition and characterized by scanning electron microscopy, X-ray diffraction, X-ray photoelectron spectroscopy, and linear sweep voltammetry. We confirmed pure (beta-PbO2 crystals were on the electrode and it had a high oxygen evolution potential. The photoactivity
J Berashevich et al.
Journal of physics. Condensed matter : an Institute of Physics journal, 25(7), 075803-075803 (2013-01-24)
The electronic properties of polycrystalline lead oxide consisting of a network of single-crystalline α-PbO platelets and the formation of native point defects in the α-PbO crystal lattice are studied using first-principles calculations. The results suggest that the polycrystalline nature of
Hui Lin et al.
Water research, 46(7), 2281-2289 (2012-03-03)
Electrochemical decomposition of environmentally persistent perfluorooctanoic acid (PFOA) in aqueous solution was investigated over Ti/SnO(2)-Sb, Ti/SnO(2)-Sb/PbO(2), and Ti/SnO(2)-Sb/MnO(2) anodes. The degradation of PFOA followed pseudo-first-order kinetics. The degradation ratios on Ti/SnO(2)-Sb, Ti/SnO(2)-Sb/PbO(2), and Ti/SnO(2)-Sb/MnO(2) anodes achieved 90.3%, 91.1%, and 31.7%
Xingwen Lu et al.
Water research, 47(3), 1353-1360 (2013-01-05)
This study quantified the effects of lead stabilization by blending lead-containing sludge into glass-ceramics through sintering with aluminum- and silica-rich precursors. Using lead oxide (PbO) to simulate lead-laden sludge under thermal conditions, the predominant PbAl(2)O(4) phase was found at temperatures
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.
联系客户支持