GF41572414

foil, 8mm disks, thickness 0.0075mm, as rolled, 99.95%

别名:

登录查看公司和协议定价


About This Item

经验公式(希尔记法):
Pt
CAS号:
分子量:
195.08
MDL號碼:
分類程式碼代碼:
12141734
PubChem物質ID:
NACRES:
NA.23

化驗

99.95%

形狀

foil

製造商/商標名

Goodfellow 415-724-14

電阻係數

10.6 μΩ-cm, 20°C

直徑× 厚度

8 mm × 0.0075 mm

bp

3827 °C (lit.)

mp

1772 °C (lit.)

密度

21.45 g/cm3 (lit.)

SMILES 字串

[Pt]

InChI

1S/Pt

InChI 密鑰

BASFCYQUMIYNBI-UHFFFAOYSA-N

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

儲存類別代碼

13 - Non Combustible Solids

水污染物質分類(WGK)

nwg

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析证书(COA)

输入产品批号来搜索 分析证书(COA) 。批号可以在产品标签上"批“ (Lot或Batch)字后找到。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

Minimally invasive makeover: platinum foil technique.
Steve Ballis et al.
Dentistry today, 29(2), 146-146 (2010-03-04)
A Medici et al.
Steroids, 66(2), 63-69 (2001-01-09)
Regioselectivity in the anodic electrochemical oxidation of cholic acid with different anodes is described. The oxidation with PbO(2) anode affords the dehydrocholic acid in quantitative yield after 22 h. 3alpha,12alpha-Dihydroxy-7-oxo-5beta-cholan-24-oic acid (59%) and 3alpha-hydroxy-7,12-dioxo-5beta-cholan-24-oic acid (51%) are obtained stopping the
Yasar F Mansour et al.
Acta odontologica Scandinavica, 64(4), 231-236 (2006-07-11)
To quantify luting cement at the crown-tooth interface of esthetic crowns fabricated using four different techniques and two methods of excess cement removal. Four methods of crown fabrication were used: the feldspathic porcelain and platinum foil technique, the feldspathic porcelain
M Schuettler et al.
Journal of neural engineering, 2(1), S121-S128 (2005-05-07)
A new method for fabrication of microelectrode arrays comprised of traditional implant materials is presented. The main construction principle is the use of spun-on medical grade silicone rubber as insulating substrate material and platinum foil as conductor (tracks, pads and
L Tröger et al.
Journal of synchrotron radiation, 8(Pt 2), 105-109 (2001-08-22)
Experimental data are presented which demonstrate the existence of a fine structure in extended X-ray absorption spectra due to interference effects in the initial photon state (piXAFS). Interference occurs between the incident electromagnetic wave and its coherently scattered waves from

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门