98.80%
形狀
foil
製造商/商標名
Goodfellow 027-055-65
電阻係數
11 μΩ-cm, 20°C
長度 × 厚度
0.5 m × 0.075 mm
bp
2270 °C (lit.)
mp
231.9 °C (lit.)
密度
7.310 g/mL at 25 °C (lit.)
SMILES 字串
[Sn]
InChI
1S/Sn
InChI 密鑰
ATJFFYVFTNAWJD-UHFFFAOYSA-N
相关类别
一般說明
For updated SDS information please visit www.goodfellow.com.
法律資訊
Product of Goodfellow
Mercury contamination removed with tin foil.
Operative dentistry, 9(3), 101-104 (1984-01-01)
Forensic science international, 134(2-3), 134-141 (2003-07-10)
Previously, electrical injuries have been suggested caused only by the concomitant heat developed during the passage of an electrical current. Recent experimental studies on fully anesthetized pigs and the study of one human case have, however, shown typical electrical alterations.
Clinical oral implants research, 22(6), 664-668 (2010-11-04)
To evaluate the necessity of three-dimensional imaging (computed tomography [CT]/cone-beam computed tomography [CBCT]) for paramedian insertion of palatal implants. Lateral radiographs and CBCT scans were performed from 18 human skulls. For lateral cephalometry, the nasal floor (right/left) and the oral
Genome biology and evolution, 7(6), 1490-1505 (2015-05-16)
We set out to investigate potential differences and similarities between the selective forces acting upon the coding and noncoding regions of five different sets of genes defined according to functional and evolutionary criteria: 1) two reference gene sets presenting accelerated
Are nickel, vanadium, silicon, fluorine, and tin essential for man? A review.
The American journal of clinical nutrition, 27(5), 515-520 (1974-05-01)
我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.
联系技术服务部门