Saltar al contenido
Merck

428043

Sigma-Aldrich

Polyethylene

low density, melt index 25 g/10 min (190°C/2.16kg)

Sinónimos:

PE

Iniciar sesiónpara Ver la Fijación de precios por contrato y de la organización


About This Item

Fórmula lineal:
H(CH2CH2)nH
Número de CAS:
Número MDL:
Código UNSPSC:
12162002
ID de la sustancia en PubChem:
NACRES:
NA.23

Nivel de calidad

Formulario

pellets

índice de fusión

25 g/10 min (190°C/2.16kg)

fuerza del impacto

45.4 J/m (Izod, ASTM D 256, −50 °C, notched)

mp

116 °C

temperatura de transición

softening point 93 °C (Vicat, ASTM D 1525)

densidad

0.925 g/mL at 25 °C

cadena SMILES

C=C

InChI

1S/C2H4/c1-2/h1-2H2

Clave InChI

VGGSQFUCUMXWEO-UHFFFAOYSA-N

¿Está buscando productos similares? Visita Guía de comparación de productos

Aplicación

Injection and blow molded toys, housewares and lids.

Características y beneficios

Good toughness, processability and appearance.

Código de clase de almacenamiento

11 - Combustible Solids

Clase de riesgo para el agua (WGK)

WGK 3

Equipo de protección personal

Eyeshields, Gloves, type N95 (US)


Elija entre una de las versiones más recientes:

Certificados de análisis (COA)

Lot/Batch Number

¿No ve la versión correcta?

Si necesita una versión concreta, puede buscar un certificado específico por el número de lote.

¿Ya tiene este producto?

Encuentre la documentación para los productos que ha comprado recientemente en la Biblioteca de documentos.

Visite la Librería de documentos

Los clientes también vieron

Flora Rendell-Bhatti et al.
Environmental pollution (Barking, Essex : 1987), 269, 115744-115744 (2020-12-02)
Microplastic pollution has become ubiquitous, affecting a wide variety of biota. Although microplastics are known to alter the development of a range of marine invertebrates, no studies provide a detailed morphological characterisation of the developmental defects. Likewise, the developmental toxicity
Lisa K McCarthy et al.
Pediatrics, 132(1), e135-e141 (2013-06-19)
Hypothermia on admission to the NICU is associated with increased mortality in preterm infants. Many newborns are hypothermic on admission despite using polyethylene bags (PBs). Using exothermic mattresses (EMs) in addition to PBs may reduce hypothermia but increase hyperthermia. We
Katharine S Woods et al.
American journal of veterinary research, 74(4), 523-529 (2013-03-28)
To compare the diagnostic quality of bronchoalveolar lavage (BAL) fluid acquired from healthy dogs by manual aspiration via polyethylene tubing (MAPT) and via suction pump aspiration (SPA) with a suction trap connection. 12 healthy adult Beagles. BAL was performed with
Agnieszka Karbownik et al.
Acta poloniae pharmaceutica, 70(2), 301-307 (2013-04-26)
The study concerned the stability of calcium folinate in concentrate in glass vials and diluted in polyethylene (PE) bags stored at 15-25 degrees C and 2-8 degrees C for up to 34 days. Original vials of calcium folinate injection (10
Nina Bloecher et al.
Biofouling, 29(3), 237-246 (2013-02-27)
The hydroid Ectopleura larynx is one of the main fouling organisms on salmon aquaculture cages in Norway; this study investigated novel surface materials and microtopographies to deter its settlement. The settlement preferences of hydroid larvae for 12 materials with wettabilities

Nuestro equipo de científicos tiene experiencia en todas las áreas de investigación: Ciencias de la vida, Ciencia de los materiales, Síntesis química, Cromatografía, Analítica y muchas otras.

Póngase en contacto con el Servicio técnico