跳转至内容
Merck

GF50035137

foil, 5m coil, thickness 0.025mm, annealed, 99.2%

别名:

登录查看公司和协议定价


About This Item

经验公式(希尔记法):
Zr
CAS号:
分子量:
91.22
MDL號碼:
分類程式碼代碼:
12141751
PubChem物質ID:
NACRES:
NA.23

化驗

99.2%

形狀

foil

製造商/商標名

Goodfellow 500-351-37

電阻係數

40 μΩ-cm, 20°C

長度 × 厚度

5 m × 0.025 mm

bp

4377 °C (lit.)

mp

1852 °C (lit.)

密度

6.5 g/mL at 25 °C (lit.)

SMILES 字串

[Zr]

InChI

1S/Zr

InChI 密鑰

QCWXUUIWCKQGHC-UHFFFAOYSA-N

正在寻找类似产品? 访问 产品对比指南

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

儲存類別代碼

4.1B - Flammable solid hazardous materials

水污染物質分類(WGK)

nwg

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析证书(COA)

输入产品批号来搜索 分析证书(COA) 。批号可以在产品标签上"批“ (Lot或Batch)字后找到。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

Daryoush Afzali et al.
Environmental monitoring and assessment, 186(6), 3523-3529 (2014-02-04)
In this study, a ternary Zr(IV) system with 2-(5-bromo-2-pyridylazo)-5-diethylaminophenol (5-Br-PADAP) and fluoride was chosen on the basis of dispersive liquid-liquid microextraction method. Zirconium was extracted into the fine droplets of dichlorobenzene as extracting solvent. These drops dispersed as a cloud
Muhammad Shahid et al.
Reviews of environmental contamination and toxicology, 221, 107-127 (2012-10-24)
Zirconium (Zr) is a transition metal that has both stable and radioactive isotopes.This metal has gained significant attention as a major pollutant of concern, partly because it has been prominent in the debate concerning the growing anthropogenic pressure on the
Oluwatayo F Ikotun et al.
Future medicinal chemistry, 3(5), 599-621 (2011-04-30)
Positron emission tomography, with its high sensitivity and resolution, is growing rapidly as an imaging technology for the diagnosis of many disease states. The success of this modality is reliant on instrumentation and the development of effective and novel targeted
Joseph R Osborne et al.
The Journal of urology, 191(5), 1439-1445 (2013-10-19)
In this pilot study we explored the feasibility of (89)Zr labeled J591 monoclonal antibody positron emission tomography of localized prostate cancer. Before scheduled radical prostatectomy 11 patients were injected intravenously with (89)Zr-J591, followed 6 days later by whole body positron
Thomas J Heyse et al.
Expert review of medical devices, 9(4), 409-421 (2012-08-22)
Polyethylene wear is a key contributor to long-term failure in total knee arthroplasty. Oxidized zirconium alloy was created as a bearing surface for total joint arthroplasty in an attempt to address this concern. Oxidized zirconium has shown considerable improvements over

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门