推荐产品
蒸汽密度
5 (vs air)
蒸汽壓力
51.7 mmHg ( 37.7 °C)
化驗
97%
形狀
liquid
折射率
n20/D 1.490 (lit.)
bp
200-201 °C (lit.)
密度
0.923 g/mL at 25 °C (lit.)
SMILES 字串
CC(C)(C)SSC(C)(C)C
InChI
1S/C8H18S2/c1-7(2,3)9-10-8(4,5)6/h1-6H3
InChI 密鑰
BKCNDTDWDGQHSD-UHFFFAOYSA-N
正在寻找类似产品? 访问 产品对比指南
一般說明
在H2O2存在下,双(乙酰丙酮)氧钒和手性席夫碱配体催化的二叔丁基二硫醚的氧化机理已有研究。
應用
二叔二硫化丁基二甲基亚砜已被用于通过对称和混合二硫化物吸附剂,制备金载薄膜。
危險聲明
危險分類
Aquatic Chronic 2
儲存類別代碼
10 - Combustible liquids
水污染物質分類(WGK)
WGK 3
閃點(°F)
143.6 °F - closed cup
閃點(°C)
62 °C - closed cup
個人防護裝備
Eyeshields, Gloves, multi-purpose combination respirator cartridge (US)
The Journal of organic chemistry, 68(1), 150-155 (2003-01-08)
The mechanism of the oxidation of di-tert-butyl disulfide (1) to the chiral thiosulfinate (2) by H(2)O(2) catalyzed by bis(acetylacetonato)oxovanadium and a chiral Schiff-base ligand (3) has been investigated. Techniques included (51)V NMR spectroscopy, solvent effects on reaction enantioselectivity, and the
Nanomaterials (Basel, Switzerland), 11(1) (2021-01-13)
Colloidal nanoparticles (NPs) have been recently spotlighted as building blocks for various nanostructured devices. Their collective properties have been exhibited by arranging them on a substrate to form assembled NPs. In particular, electrophoretic deposition (EPD) is an emerging fabrication method
Contact angle goniometry, ellipsometry, XPS, and TOF-SIMS analysis of gold-supported, mixed self-assembled monolayers formed from mixed dialkyl disulfides.
Langmuir, 10(3), 761-766 (1994)
ACS nano, 12(8), 7803-7811 (2018-07-10)
Heterogeneous copper sulfide based nanostructures have attracted intense attention based on their potential to combine the plasmonic properties of copper-deficient copper sulfides with properties of other semiconductors and metals. In general, copper sulfides are versatile platforms for production of other