735817
Polypyrrole-block-poly(caprolactone)
0.3-0.7 wt. % (dispersion in nitromethane), contains p-toluenesulfonate as dopant
Synonym(s):
Biotron PP-NM, PCL-block-PPy
Sign Into View Organizational & Contract Pricing
All Photos(1)
About This Item
Recommended Products
form
liquid (dispersion)
Quality Level
contains
p-toluenesulfonate as dopant
composition
Biotron PP polymer, 0.3-0.7 wt. %
ethanol, 4-8 wt. %
nitromethane, 90-95 wt. %
concentration
0.3-0.7 wt. % (dispersion in nitromethane)
conductivity
10-40 S/cm (bulk)
General description
Sheet resistance, spin cast thin films: 10,000-50,000 Ohms/sq
Average transmittance: 70-90%
Biodegradble conducting polymer for bomedical applications. PCL diol blocks have average molecular weight 2000 and PPy block have an average molecular weight of 4000 with a 25% doping level. Good biocompatibility with expected weight loss of 40% at 200 days in pH=7 buffer.
Average transmittance: 70-90%
Biodegradble conducting polymer for bomedical applications. PCL diol blocks have average molecular weight 2000 and PPy block have an average molecular weight of 4000 with a 25% doping level. Good biocompatibility with expected weight loss of 40% at 200 days in pH=7 buffer.
Application
Thin films can be prepared by spin casting the nitromethane dispersion at 1000 rpm. To spin coat a thin film at 1000 RPM, 30 seconds to 1 minute is usually enough time to spread this dispersion. Thicker and more conducting films can be prepared by air spraying the dispersion on a substrate. Any substrate that is compatible can be used. Sprayed films can be dried at 30-40 °C, then pressed between two polished dye plates at 1000-10,000 psi to increase film density, strength and scratch resistance. The drying time of the air sprayed film depends on the thickness of the prepared film. Try weighing the sample periodically during drying.
Features and Benefits
The block copolymer structure renders the conducting polymer polypyrrole dispersible in organic solvents and biodegradable.
Caution
Store this product at room temperature (do not refrigerate or freeze). Severe settling and separation will normally occur. Agitate, sonicate, and filter prior to use. A plug of glass wool in a pipette can be used for easy filtration. The shelf life of this product will vary depending on how it is stored and handled. Product should be discarded if heavy aggregation occurs, or if sonication / filtering are inadequate to produce a good casting solution. When spray coating is used, the user should take every precaution necessarily to prevent exposure to solvent vapors from this product
Other Notes
Will settle over time. Must be sonicated before use
Legal Information
Signal Word
Danger
Hazard Statements
Precautionary Statements
Hazard Classifications
Acute Tox. 4 Inhalation - Acute Tox. 4 Oral - Carc. 2 - Flam. Liq. 2 - Repr. 2
Storage Class Code
3 - Flammable liquids
WGK
WGK 2
Flash Point(F)
66.9 °F
Flash Point(C)
19.4 °C
Choose from one of the most recent versions:
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Customers Also Viewed
Synergic effect in electrical conductivity using a combination of two fillers in PVDF hybrids composites.
European Polymer Journal, 49(10), 3318-3327 (2013)
Polypropylene composites for polymer electrolyte membrane fuel cell bipolar plates.
Macromolecular Symposia, 264(1) (2008)
Materials for Bioelectronic and
Biomedical Applications
Biomedical Applications
Material Matters, 8(1) null
Chemical Synthesis and Morphology of b?Naphthalene Sulfonic Acid-Doped Polypyrrole Micro/Nanotube.
Fullerenes, Nanotubes, and Carbon Nanostructures, 14 (2006)
Soluble conducting polypyrrole doped with DBSA?CSA mixed acid
Journal of Applied Polymer Science, 68(8), 1277-1284 (1998)
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service