Highly conductive and stretchable polymer composites based on graphene/MWCNT network.

Chemical communications (Cambridge, England) (2013-01-22)
Mengting Chen, Tao Tao, Ling Zhang, Wei Gao, Chunzhong Li
์ดˆ๋ก

We have manufactured a highly conductive and stretchable composite by backfilling a preformed graphene/MWCNT aerogel with poly(dimethylsiloxane) (PDMS). The electrical conductivity of our product can reach 2.8 S cm(-1) with only 1.3 wt% graphene/MWCNT loading, and remains constant after 100 times repeated stretching by 20% and 5000 times bending.

MATERIALS
์ œํ’ˆ ๋ฒˆํ˜ธ
๋ธŒ๋žœ๋“œ
์ œํ’ˆ ์„ค๋ช…

Sigma-Aldrich
Silicone oil, viscosity 100 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 50 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 60,000 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 500 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 20 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 350 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 10,000 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 100,000 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 30,000 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 10 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, viscosity 1,000 cSt (25 ยฐC)
Silicone oil, for melting point and boiling point apparatuses
Sigma-Aldrich
Silicone oil, viscosity 5 cSt (25 ยฐC)
Sigma-Aldrich
Silicone oil, for oil baths (from −50ยฐC to +200ยฐC)