GF33254793
Platinum
foil, 25x25mm, thickness 0.1mm, as rolled, 99.95%
Synonym(s):
Platinum, PT000261
Sign Into View Organizational & Contract Pricing
All Photos(2)
About This Item
Recommended Products
Assay
99.95%
form
foil
manufacturer/tradename
Goodfellow 332-547-93
resistivity
10.6 μΩ-cm, 20°C
size × thickness
25x25 mm × 0.1 mm
bp
3827 °C (lit.)
mp
1772 °C (lit.)
density
21.45 g/cm3 (lit.)
SMILES string
[Pt]
InChI
1S/Pt
InChI key
BASFCYQUMIYNBI-UHFFFAOYSA-N
General description
For updated SDS information please visit www.goodfellow.com.
Legal Information
Product of Goodfellow
Storage Class Code
13 - Non Combustible Solids
WGK
nwg
Flash Point(F)
Not applicable
Flash Point(C)
Not applicable
Certificates of Analysis (COA)
Search for Certificates of Analysis (COA) by entering the products Lot/Batch Number. Lot and Batch Numbers can be found on a product’s label following the words ‘Lot’ or ‘Batch’.
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Minimally invasive makeover: platinum foil technique.
Dentistry today, 29(2), 146-146 (2010-03-04)
Acta odontologica Scandinavica, 64(4), 231-236 (2006-07-11)
To quantify luting cement at the crown-tooth interface of esthetic crowns fabricated using four different techniques and two methods of excess cement removal. Four methods of crown fabrication were used: the feldspathic porcelain and platinum foil technique, the feldspathic porcelain
Child's nervous system : ChNS : official journal of the International Society for Pediatric Neurosurgery, 19(4), 211-216 (2003-04-26)
Our hypothesis was that a neurocranial suture autograft will, when shielded from dura, grow and be incorporated into the calvarium. Growth was monitored by marker separation in three isohistogenic groups of rabbits, between postnatal days 9 and 90. In order
Using platinum foil techniques to create natural tooth color.
Practical procedures & aesthetic dentistry : PPAD, 20(8), 479-481 (2008-11-11)
Conference proceedings : ... Annual International Conference of the IEEE Engineering in Medicine and Biology Society. IEEE Engineering in Medicine and Biology Society. Annual Conference, 2009, 1612-1615 (2009-12-08)
An easy and fast method for fabrication of neural electrode arrays is the patterning of platinum foil and spin-on silicone rubber using a laser. However, the mechanical flexibility of such electrode arrays is limited by the integrated tracks that connect
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service