蒸気圧
<0.01 mmHg ( 537.2 °C)
アッセイ
99.9%
形状
tubes
自己発火温度
572 °F
メーカー/製品名
Goodfellow 374-786-83
抵抗性
13.5 μΩ-cm, 20°C
L ×壁厚
100 mm × 0.3 mm
外径 × 内径
5.0 mm × 4.4 mm
bp
5425 °C (lit.)
mp
2996 °C (lit.)
密度
16.69 g/cm3 (lit.)
SMILES記法
[Ta]
InChI
1S/Ta
InChI Key
GUVRBAGPIYLISA-UHFFFAOYSA-N
詳細
For updated SDS information please visit www.goodfellow.com.
法的情報
Goodfellow製品
最新バージョンのいずれかを選択してください:
The Journal of arthroplasty, 29(4), 831-835 (2013-10-09)
This study compared the corrosion behavior of tantalum-coated cobalt-chromium modular necks with that of titanium alloy modular necks at their junction to titanium-alloy femoral stem. Tests were performed in a dry assembly and two wet assemblies, one contaminated with calf
Zhongguo gu shang = China journal of orthopaedics and traumatology, 26(7), 617-620 (2013-10-19)
Incorrect treatment for femur head necrosis can cause collapse of femoral head and tresult in severe harm for the patients (especially for the patient with middle-aged and young). The structure and mechanics characteristics of tantalum rod is similar to bone
[Tantalum dust as a contrast substance for laryngography and bronchography (a review of the literature)].
Vestnik rentgenologii i radiologii, (1)(1), 77-79 (1981-01-01)
Clinical use of porous tantalum in complex primary total knee arthroplasty.
American journal of orthopedics (Belle Mead, N.J.), 38(10), 526-530 (2009-12-17)
Metallosis and elevated serum levels of tantalum following failed revision hip arthroplasty--a case report.
Acta orthopaedica, 85(6), 677-680 (2014-08-21)
ライフサイエンス、有機合成、材料科学、クロマトグラフィー、分析など、あらゆる分野の研究に経験のあるメンバーがおります。.
製品に関するお問い合わせはこちら(テクニカルサービス)