Tantalum

foil, light tested, 150x150mm, thickness 0.075mm, annealed, 99.9%

Sinónimos:

Tantalum, TA000384, Ta

Iniciar sesiónpara Ver la Fijación de precios por contrato y de la organización


About This Item

Fórmula empírica (notación de Hill):
Ta
Número de CAS:
Peso molecular:
180.95
Número MDL:
Código UNSPSC:
12141741
ID de la sustancia en PubChem:
NACRES:
NA.23

presión de vapor

<0.01 mmHg ( 537.2 °C)

Ensayo

99.9%

Formulario

foil

temp. de autoignición

572 °F

fabricante / nombre comercial

Goodfellow 795-431-10

resistividad

13.5 μΩ-cm, 20°C

tamaño × grosor

150 x 150 mm × 0.075 mm

bp

5425 °C (lit.)

mp

2996 °C (lit.)

densidad

16.69 g/cm3 (lit.)

cadena SMILES

[Ta]

InChI

1S/Ta

Clave InChI

GUVRBAGPIYLISA-UHFFFAOYSA-N

Descripción general

For updated SDS information please visit www.goodfellow.com.

Información legal

Product of Goodfellow

Elija entre una de las versiones más recientes:

Certificados de análisis (COA)

Lot/Batch Number

It looks like we've run into a problem, but you can still download Certificates of Analysis from our Documentos section.

Si necesita más asistencia, póngase en contacto con Atención al cliente

¿Ya tiene este producto?

Encuentre la documentación para los productos que ha comprado recientemente en la Biblioteca de documentos.

Visite la Librería de documentos

Tantalum foil cuffs in peripheral nerve surgery.
E E CLIFFTON
Surgery, 23(3), 507-514 (1948-03-01)
Tantalum foil pegs.
E MAXWELL
American journal of ophthalmology, 34(3), 444-444 (1951-03-01)
Yingxun Du et al.
Journal of hazardous materials, 225-226, 21-27 (2012-05-23)
In order to overcome the limitation of the application of nanoparticles, tantalum (oxy)nitrides nanotube arrays on a Ta foil were synthesized and introduced in vis (visible light)-Fenton-like system to enhance the degradation of atrazine. At first, the anodization of tantalum
J G Sen Gupta
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
Radmila Panajotovic et al.
Radiation research, 165(4), 452-459 (2006-04-04)
We determined effective cross sections for production of single-strand breaks (SSBs) in plasmid DNA [pGEM 3Zf(-)] by electrons of 10 eV and energies between 0.1 and 4.7 eV. After purification and lyophilization on a chemically clean tantalum foil, dry plasmid

Nuestro equipo de científicos tiene experiencia en todas las áreas de investigación: Ciencias de la vida, Ciencia de los materiales, Síntesis química, Cromatografía, Analítica y muchas otras.

Póngase en contacto con el Servicio técnico