264059
Indium
foil, thickness 0.127 mm, 99.99% trace metals basis
Synonym(s):
Indium element
Sign Into View Organizational & Contract Pricing
All Photos(1)
About This Item
Recommended Products
vapor pressure
<0.01 mmHg ( 25 °C)
Quality Level
Assay
99.99% trace metals basis
form
foil
resistivity
8.37 μΩ-cm
thickness
0.127 mm
mp
156.6 °C (lit.)
density
7.3 g/mL at 25 °C (lit.)
SMILES string
[In]
InChI
1S/In
InChI key
APFVFJFRJDLVQX-UHFFFAOYSA-N
Looking for similar products? Visit Product Comparison Guide
Application
Indium foil is thermal interface material with high conductance that is used in cryogenics. It can also be used as indium vapor source for the preparation of indium nitride nanowires on a silicon substrate. It may also be used in the time of flight secondary ion mass spectroscopy (ToF-SIMS) for the analysis of powder samples.
Quantity
2.3 g = 50 × 50 mm; 9.2 g = 100 × 100 mm
Signal Word
Danger
Hazard Statements
Precautionary Statements
Hazard Classifications
STOT RE 1 Inhalation
Target Organs
Lungs
Storage Class Code
6.1C - Combustible acute toxic Cat.3 / toxic compounds or compounds which causing chronic effects
WGK
WGK 1
Flash Point(F)
Not applicable
Flash Point(C)
Not applicable
Personal Protective Equipment
dust mask type N95 (US), Eyeshields, Gloves
Choose from one of the most recent versions:
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Cryogen-free operation of 10 V programmable Josephson voltage standards
IEEE Transactions on Applied Superconductivity, 23(3) (2012)
Characteristic fragment ions from lignin and polysaccharides in ToF-SIMS
Wood Science and Technology, 45(4), 767-785 (2011)
Selective-area growth of indium nitride nanowires on gold-patterned Si (100) substrates
Applied Physics Letters, 81(1), 22-24 (2002)
Chemical communications (Cambridge, England), 49(22), 2237-2239 (2013-02-12)
A reduced graphene oxide (RGO)-ZnIn(2)S(4) nanosheet composite was successfully synthesized via an in situ controlled growth process. The as-obtained RGO-ZnIn(2)S(4) composite showed excellent visible light H(2) production activity in the absence of noble metal cocatalysts.
Optics express, 21 Suppl 1, A1-A6 (2013-02-15)
A wing-type imbedded electrodes was introduced into the lateral light emitting diode configuration (WTIE-LEDs) to reduce the effect of light shading of electrode in conventional sapphire-based LEDs (CSB-LEDs). The WTIE-LEDs with double-side roughened surface structures not only can eliminate the
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service