Structural evolution of an intermetallic Pd-Zn catalyst selective for propane dehydrogenation.

Physical chemistry chemical physics : PCCP (2015-03-21)
James R Gallagher, David J Childers, Haiyan Zhao, Randall E Winans, Randall J Meyer, Jeffrey T Miller
RÉSUMÉ

We report the structural evolution of Pd-Zn alloys in a 3.6% Pd-12% Zn/Al2O3 catalyst which is selective for propane dehydrogenation. High signal-to-noise, in situ synchrotron X-ray diffraction (XRD) was used quantitatively, in addition to in situ diffuse-reflectance infrared Fourier transform spectroscopy (DRIFTS) and extended X-ray absorption fine structure (EXAFS) to follow the structural changes in the catalyst as a function of reduction temperature. XRD in conjunction with DRIFTS of adsorbed CO indicated that the β1-PdZn intermetallic alloy structure formed at reduction temperatures as low as 230 °C, likely first at the surface, but did not form extensively throughout the bulk until 500 °C which was supported by in situ EXAFS. DRIFTS results suggested there was little change in the surfaces of the nanoparticles above 325 °C. The intermetallic alloy which formed was Pd-rich at all temperatures but became less Pd-rich with increasing reduction temperature as more Zn incorporated into the structure. In addition to the β1-PdZn alloy, a solid solution phase with face-center cubic structure (α-PdZn) was present in the catalyst, also becoming more Zn-rich with increasing reduction temperature.

MATÉRIAUX
Référence du produit
Marque
Description du produit

Sigma-Aldrich
Oxyde d′aluminium, activated, basic, Brockmann I
Sigma-Aldrich
Oxyde d′aluminium, activated, neutral, Brockmann I
Sigma-Aldrich
Oxyde d′aluminium, powder, 99.99% trace metals basis
Sigma-Aldrich
Oxyde d′aluminium, activated, acidic, Brockmann I
Sigma-Aldrich
Oxyde d′aluminium, nanopowder, <50 nm particle size (TEM)
Sigma-Aldrich
Oxyde d′aluminium, powder, primarily α phase, ≤10 μm avg. part. size, 99.5% trace metals basis
Sigma-Aldrich
Aluminum oxide, nanoparticles, <50 nm particle size (DLS), 20 wt. % in isopropanol
Sigma-Aldrich
Oxyde d′aluminium, pellets, 3 mm
Sigma-Aldrich
Oxyde d′aluminium, Corundum, α-phase, -100 mesh
Sigma-Aldrich
Oxyde d′aluminium, nanopowder, 13 nm primary particle size (TEM), 99.8% trace metals basis
Sigma-Aldrich
Oxyde d′aluminium, fused, powder, primarily α-phase, -325 mesh
Sigma-Aldrich
Oxyde d′aluminium, 99.997% trace metals basis
Sigma-Aldrich
Oxyde d′aluminium, pore size 58 Å, ~150 mesh
Sigma-Aldrich
Oxyde d′aluminium, Type WN-6, Neutral, Activity Grade Super I
Sigma-Aldrich
Aluminum oxide, nanoparticles, 30-60 nm particle size (TEM), 20 wt. % in H2O
Sigma-Aldrich
Oxyde d′aluminium, fused, powder, primarily α-phase, 100-200 mesh
Sigma-Aldrich
Oxyde d′aluminium, nanowires, diam. × L 2-6 nm × 200-400 nm
Sigma-Aldrich
Aluminum oxide, mesostructured, MSU-X (wormhole), average pore size 3.8 nm
Sigma-Aldrich
Oxyde d′aluminium, single crystal substrate, <0001>
Sigma-Aldrich
Oxyde d′aluminium, activated, neutral, Brockmann I, free-flowing, Redi-Dri
Sigma-Aldrich
Oxyde d′aluminium, activated, acidic, Brockmann I, free-flowing, Redi-Dri