659401
Poly(styrene-ran-ethylene), sulfonated, cross-linkable solution
About This Item
Composition
styrene, 76 wt. %
sulfonated stryene units, 32-38%
vinyl silane cross-linking agent, <0.5%
Concentration
5 wt. % in 1-propanol
Indice de réfraction
n20/D 1.384
Conductivité
0.1184 S/cm (The ionic conductivity can increase up to 50% when heating from RT to 67°C)
Point d'ébullition
57-60 °C
Densité
0.85 g/mL at 25 °C
Application
Notes préparatoires
1. Concentrate solution to 600 centapoise viscosity (typically 6-9 wt.% polymer).
2. Preheat the casting surface to 35 °C. A clean, flat PTFE-coated glass surface is recommended.
3. Secure a silicone release liner to the casting surface.
4. Place a small drop of the polymer solution on the release liner.
5. Draw the polymer solution down the release liner.
6. Dry the film for 30 min. For controlled evaporation it is recommended to cover surface with aluminum foil that has been perforated with small pinholes.
Certificats d'analyse (COA)
Recherchez un Certificats d'analyse (COA) en saisissant le numéro de lot du produit. Les numéros de lot figurent sur l'étiquette du produit après les mots "Lot" ou "Batch".
Déjà en possession de ce produit ?
Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.
Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..
Contacter notre Service technique