Effect of nanoconfinement on polymer dynamics: surface layers and interphases.

Physical review letters (2013-03-26)
M Krutyeva, A Wischnewski, M Monkenbusch, L Willner, J Maiz, C Mijangos, A Arbe, J Colmenero, A Radulescu, O Holderer, M Ohl, D Richter
RÉSUMÉ

We present neutron spin echo experiments that address the much debated topic of dynamic phenomena in polymer melts that are induced by interacting with a confining surface. We find an anchored surface layer that internally is highly mobile and not glassy as heavily promoted in the literature. The polymer dynamics in confinement is, rather, determined by two phases, one fully equal to the bulk polymer and another that is partly anchored at the surface. By strong topological interaction, this phase confines further chains with no direct contact to the surface. These form the often invoked interphase, where the full chain relaxation is impeded through the interaction with the anchored chains.

MATÉRIAUX
Référence du produit
Marque
Description du produit

Sigma-Aldrich
Huile de silicone, viscosity 10 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 5 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 20 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 100 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, for oil baths (from −50°C to +200°C)
Sigma-Aldrich
Huile de silicone, viscosity 1,000 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 350 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 500 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 50 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 10,000 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 60,000 cSt (25 °C)
Huile de silicone, for melting point and boiling point apparatuses
Sigma-Aldrich
Huile de silicone, viscosity 100,000 cSt (25 °C)
Sigma-Aldrich
Huile de silicone, viscosity 30,000 cSt (25 °C)