GF55367185
Tantalum
foil, 0.2m coil, thickness 0.01mm, 99.9%
Synonyme(s) :
Tantalum, TA000290, Ta
Se connecterpour consulter vos tarifs contractuels et ceux de votre entreprise/organisme
About This Item
Pression de vapeur
<0.01 mmHg ( 537.2 °C)
Pureté
99.9%
Forme
foil
Température d'inflammation spontanée
572 °F
Fabricant/nom de marque
Goodfellow 553-671-85
Résistivité
13.5 μΩ-cm, 20°C
L × épaisseur
0.2 m × 0.01 mm
Point d'ébullition
5425 °C (lit.)
Pf
2996 °C (lit.)
Densité
16.69 g/cm3 (lit.)
Chaîne SMILES
[Ta]
InChI
1S/Ta
Clé InChI
GUVRBAGPIYLISA-UHFFFAOYSA-N
Catégories apparentées
Description générale
For updated SDS information please visit www.goodfellow.com.
Informations légales
Product of Goodfellow
Certificats d'analyse (COA)
Recherchez un Certificats d'analyse (COA) en saisissant le numéro de lot du produit. Les numéros de lot figurent sur l'étiquette du produit après les mots "Lot" ou "Batch".
Déjà en possession de ce produit ?
Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.
Radiation research, 165(4), 452-459 (2006-04-04)
We determined effective cross sections for production of single-strand breaks (SSBs) in plasmid DNA [pGEM 3Zf(-)] by electrons of 10 eV and energies between 0.1 and 4.7 eV. After purification and lyophilization on a chemically clean tantalum foil, dry plasmid
Applied optics, 31(22), 4397-4404 (1992-08-01)
A simple four-element fused-silica lens is presented that has a focal length of 31.2 mm and a relative aperture of f/1 for use as a focusing lens for deep UV laser processing. The curvature of the lens is designed with
Tantalum foil pegs.
American journal of ophthalmology, 34(3), 444-444 (1951-03-01)
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..
Contacter notre Service technique