Accéder au contenu
Merck
Toutes les photos(1)

Principaux documents

767514

Sigma-Aldrich

Tantalum

sputtering target, diam. × thickness 2.00 in. × 0.25 in., 99.95% trace metals basis

Synonyme(s) :

Ta

Se connecterpour consulter vos tarifs contractuels et ceux de votre entreprise/organisme


About This Item

Formule empirique (notation de Hill) :
Ta
Numéro CAS:
Poids moléculaire :
180.95
Numéro CE :
Numéro MDL:
Code UNSPSC :
12352103
ID de substance PubChem :
Nomenclature NACRES :
NA.23

Pression de vapeur

<0.01 mmHg ( 537.2 °C)

Essai

99.95% trace metals basis

Forme

foil

Température d'inflammation spontanée

572 °F

Pertinence de la réaction

core: tantalum

Résistivité

13.5 μΩ-cm, 20°C

Diam. × épaisseur

2.00 in. × 0.25 in.

pb

5425 °C (lit.)

Pf

2996 °C (lit.)

Densité

16.69 g/cm3 (lit.)

Chaîne SMILES 

[Ta]

InChI

1S/Ta

Clé InChI

GUVRBAGPIYLISA-UHFFFAOYSA-N

Application

Sputtering is a process whereby atoms are ejected from a solid target material due to bombardment of the target by energetic particles. The extreme miniaturization of components in the semiconductor and electronics industry requires high purity sputtering targets for thin film deposition.

Code de la classe de stockage

11 - Combustible Solids

Classe de danger pour l'eau (WGK)

nwg

Point d'éclair (°F)

Not applicable

Point d'éclair (°C)

Not applicable


Faites votre choix parmi les versions les plus récentes :

Certificats d'analyse (COA)

Lot/Batch Number

It looks like we've run into a problem, but you can still download Certificates of Analysis from our Documents section.

Si vous avez besoin d'assistance, veuillez contacter Service Clients

Déjà en possession de ce produit ?

Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.

Consulter la Bibliothèque de documents

Kostantinidis; S.;
The European Physical Journal - Applied Physics, 56(2), 24002/1-24002/1 (2011)
Helmersson; U.;
Thin Solid Films, 513(1-2), 1-1 (2006)
Xiao-kang Tang et al.
Zhongguo gu shang = China journal of orthopaedics and traumatology, 26(7), 617-620 (2013-10-19)
Incorrect treatment for femur head necrosis can cause collapse of femoral head and tresult in severe harm for the patients (especially for the patient with middle-aged and young). The structure and mechanics characteristics of tantalum rod is similar to bone
Ulrich Dorn et al.
The Journal of arthroplasty, 29(4), 831-835 (2013-10-09)
This study compared the corrosion behavior of tantalum-coated cobalt-chromium modular necks with that of titanium alloy modular necks at their junction to titanium-alloy femoral stem. Tests were performed in a dry assembly and two wet assemblies, one contaminated with calf
[Tantalum dust as a contrast substance for laryngography and bronchography (a review of the literature)].
R M Rabinovich
Vestnik rentgenologii i radiologii, (1)(1), 77-79 (1981-01-01)

Articles

Nanocomposite Coatings with Tunable Properties Prepared by Atomic Layer Deposition

Spintronics offer breakthroughs over conventional memory/logic devices with lower power, leakage, saturation, and complexity.

The properties of many devices are limited by the intrinsic properties of the materials that compose them.

Questions

Reviews

No rating value

Active Filters

Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..

Contacter notre Service technique