콘텐츠로 건너뛰기
Merck
  • Synthesis of elastic biodegradable polyesters of ethylene glycol and butylene glycol from sebacic acid.

Synthesis of elastic biodegradable polyesters of ethylene glycol and butylene glycol from sebacic acid.

Acta biomaterialia (2012-04-24)
Hyung-seok Park, Jung-a Seo, Hye-Young Lee, Hae-Won Kim, Ivan B Wall, Myoung-Seon Gong, Jonathan C Knowles
초록

High molecular weight biodegradable polyesters were prepared from sebacic acid, ethylene glycol and butylene glycol through a simple non-solvent polycondensation with a low toxicity catalyst. The successful synthesis of the polyesters was confirmed by gel permeation chromatography, (1)H-nuclear magnetic resonance and Fourier transform-infrared spectroscopies and differential scanning calorimetry. The degradation tests were performed at 37 °C in phosphate buffer solution (pH 7.4) and showed a mass loss of ~5% over 12 weeks compared with only 2% for polycaprolactone (PCL). Reverse transcription polymerase chain reaction results following culture of osteoblasts on the polymer surface showed that poly(ethylene sebacate) and poly(butylene sebacate) films were optimal for osteoblast formation in terms of Runx 2 and osteocalcin gene expression.

MATERIALS
제품 번호
브랜드
제품 설명

Sigma-Aldrich
Sebacic acid, ≥95.0% (GC)
Sigma-Aldrich
Sebacic acid, 99%