Renewable Isohexide-Based, Hydrolytically Degradable Poly(silyl ether)s with High Thermal Stability.

ChemSusChem (2018-06-30)
Srikanth Vijjamarri, Marianne Hull, Edward Kolodka, Guodong Du
RÉSUMÉ

Several degradable poly(silyl ether)s (PSEs) have been synthesized by dehydrogenative cross-coupling between bio-based 1,4:3,6-dianhydrohexitols (isosorbide and isomannide) and commercially available hydrosilanes. An air-stable manganese salen nitrido complex [MnV N(salen-3,5-tBu2 )] was employed as the catalyst. High-molecular-weight polymer was obtained from isosorbide and diphenylsilane (Mn up to 17000 g mol-1 ). Thermal analysis showed that these PSEs possessed high thermal stability with thermal decomposition temperatures (T-5 % ) of 347-446 °C and glass transition temperatures of 42-120 °C. Structure-property analysis suggested that steric bulk and molecular weight have a significant influence to determine the thermal properties of synthesized polymers. Importantly, these polymers were degraded effectively to small molecules under acidic and basic hydrolysis conditions.

MATÉRIAUX
Référence du produit
Marque
Description du produit

Sigma-Aldrich
1,4:3,6-Dianhydro-D-mannitol, 95%